Volume 10 (2013)
Proceedings of
the 4th Japan-China Workshop
on Fusion-Related Tritium Science and Technology
May 9–11, 2012, Toyama, Japan
(Published 12 February 2013)
- COVER :
(759Kbytes)
- INDEX :
( 50Kbytes)
- PREFACE :
( 51Kbytes)
- pp.001-006 :
Improvement of Hydrogen Isotope Release on Lithium Orthosilicate Ceramic Pebble
by Catalytic Metals
Chengjian XIAO, Chunmei KANG, Xingbi REN, Xiaoling GAO, Xiaojun CHEN,
Heyi WANG and Xiaolin WANG
(500Kbytes)
- pp.007-011 :
Effects of Li4TiO4 Structure on Tritium Release Kinetics from Lithium-Enriched Li2+xTiO3
Makoto KOBAYASHI, Kiyotaka KAWASAKI, Katsuyoshi TATENUMA,
Masanori HARA, Masao MATSUYAMA, Toshiyuki FUJII, Hajimu YAMANA,
Yasuhisa OYA and Kenji OKUNO
(342Kbytes)
- pp.012-017 :
Release Behavior of Hydrogen Isotopes in Li2TiO3 Pellet
Deqiong ZHU, Takuji ODA and Satoru TANAKA
(1.3Mbytes)
- pp.018-021 :
Mass Loss of Li2TiO3 Pebbles in Atmosphere Containing Hydrogen
Hideaki KASHIMURA, Masabumi NISHIKAWA, Kazunari KATAYAMA,
Shohei MATSUDA, Satoshi FUKADA, Tsuyoshi HOSHINO
(889Kbytes)
- pp.022-026 :
Flibe-Tritium Research for Fission or Fusion Reactors at Kyushu University
Satoshi FUKADA
(701Kbytes)
- pp.027-032 :
Experimental and Computational Studies on Tritium Permeation Mechanism in Erbium Oxide
Wei MAO, Takumi CHIKADA, Akihiro SUZUKI,
Takayuki TERAI and Kenji YAMAGUCHI
(549Kbytes)
- pp.033-035 :
Solubility of Hydrogen Isotopes in Zirconia Ceramics
Kenichi HASHIZUME, Kosuke OGATA, Satoshi AKAMARU and Yuji HATANO
(384Kbytes)
- pp.036-041 :
Numerical Simulation of Detritiation System for NIFS with Commercial Catalyst and Adsorbent
Kenzo MUNAKATA, Keisuke HARA, Takahiko SUGIYAMA, Kenji KOTOH, Masahiro TANAKA and Tatsuhiko UDA
(401Kbytes)
- pp.042-048 :
Effects of La2O3, Cu and Fe Addition on the Catalytic Performance of Ni-SiO2 Catalysts for Methane Decomposition
Heyi WANG, Wenhua WANG, Yong YANG and Shuming PENG
(1.0Mbytes)
- pp.049-053 :
Measurement of Tritium Distribution in Nickel and Vanadium by Means of a Combined Technique of an Imaging Plate and Thin Absorbers
Hiroko YOSHIDA-OHUCHI, Yuji HATANO, Akram MOHAMMADI and Takao KAWANO
(770Kbytes)
- pp.054-063 :
The R&D Status of ITER SDS
Sei-Hun YUN, Chang Shuk KIM, Min Ho CHANG, Hyun-Goo KANG, Seungyon CHO, Hyun Gon LEE, Ki Jung JUNG, Hongsuk CHUNG,
Dae Seo KOO, Kyu-Min SONG, Soon-Hwan SHON and Duk Jin KIM
(8.5Mbytes)
- pp.064-070 :
Trapping of Tritium by Stainless Steel Exposed to Plasmas in Experimental Campaigns of LHD
Masao MATSUYAMA, Shinsuke ABE, Kiyohiko NISHIMURA, Yasushi ONO, Yasuhisa OYA, Kenji OKUNO, Tomoaki HINO and Akio SAGARA
(523Kbytes)
- pp.071-075 :
Simulating Tritium Retention in Tungsten with a Multiple Trap Model in the TMAP Code
Brad J. MERRILL, Masashi SHIMADA and Paul W. HUMRICKHOUSE
(446Kbytes)
- pp.076-080 :
Implantation Energy Dependence on Deuterium Retention Behaviors for the Carbon Implanted Tungsten
Yasuhisa OYA, Makoto KOBAYASHI, Naoaki YOSHIDA, Naoko ASHIKAWA, Akio SAGARA, Yuji HATANO and Kenji OKUNO
(559Kbytes)
- pp.081-084 :
Tritium Distribution on the Tungsten Surface Exposed to Deuterium Plasma and then to Tritium Gas
Kanetsugu ISOBE, Vladimir Kh. ALIMOV, Akira TAGUCHI, Makiko SAITO, Yuji TORIKAI, Yuji HATANO and Toshihiko YAMANISHI
(793Kbytes)
- pp.085-088 :
Study on Plasma-Tungsten Surface Interactions Using the New Experimental Device EXPRESS
Ryo MIURA, Tetsuo FUJISHIMA, Yuto MIYAHARA, Tomohisa TAGUCHI, Masahiro TANAKA, Akio SAGARA,Yasuhisa OYA and Kenji OKUNO
(356Kbytes)
- pp.089-093 :
Hydrogen Incorporation into Tungsten Deposits Growing under Hydrogen and Argon Mixed Plasma
Kazunari KATAYAMA, Yasuhito OHNISHI, Satoshi FUKADA and Masabumi NISHIKAWA
(507Kbytes)
- pp.094-097 :
Hydrogen Storage Properties of Nanocrystalline Mg2Ni Based Alloys Prepared by Ball-Milling
Yifu XIONG, Jingwen BA, Wuwen QING and Wenyong JING
(350Kbytes)
- pp.098-101 :
Hydrogen Generation Property on the Surface of Plasma Sintered Be12Ti
Kohei WADA, Kenzo MUNAKATA, Yusuke AKIMOTO, Haruki TAKEDA, Jae-Hwan KIM, Daisuke WAKAI, Kazuo YONEHARA and Masaru NAKAMICHI
(653Kbytes)