Volume 6, 1202005 (2011)
Rapid Communications
- Faculty of Engineering, Aichi Institute of Technology, Toyota 470-0392, Japan
Abstract
One of the serious concerns for tungsten materials in fusion devices is the radiation defects caused by helium plasma irradiation, while the helium is one of fusion products. Fiber-formed nanostructure is worried to have a possible weakness against the plasma heat flux and may destroy the reflectivity as an optical mirror. In this communication an interesting method for a recovery of such a tungsten surface is shown.
Keywords
plasma-facing material, tungsten surface, nanostructure, recovery of surface flatness, helium defect, argon plasma
Full Text
References
- [1] S. Takamura, N. Ohno, D. Nishijima and S. Kajita, Plasma Fusion Res. 1, 051 (2006).
- [2] M.J. Baldwin and D.P. Doerner, Nucl. Fusion 48, 035001 (2008).
- [3] S. Kajita, S. Takamura, N. Ohno, D. Nishijima, H. Iwakiri and N. Yoshida, Nucl. Fusion 47, 1358 (2007).
- [4] S. Takamura, T. Miyamoto and N. Ohno, Plasma Fusion Res. 5, 039 (2010).
- [5] S. Takamura et al., J. Nucl. Mater. (2011), doi: 10.1016/j.jnucmat.2010.12.021
- [6] M.Y. Ye, S. Takamura and N. Ohno, J. Nucl. Mater. 241-243, 1243 (1997).
- [7] D. Nishijima, M.Y. Ye, N. Ohno and S. Takamura, J. Nucl. Mater. 329-333, 1029 (2004).
This paper may be cited as follows:
Shuichi TAKAMURA and Takanori MIYAMOTO, Plasma Fusion Res. 6, 1202005 (2011).